  1. How come I can't get decals to work?!?!?!

    Buy a toner cartridge from Ganson.com. They make the highest iron content toner available. Used for checks and banking, it is called a MICR toner cartridge (magnetic ink character recognition). When I told them I was using it for ceramics they were VERY helpful and understood exactly what my needs were. My decals have been coming out really great since using their product.
×