  1. coloured slips

    thanks ill try these - martin
  2. coloured slips

    Hi Im new to pottery but have taken to using oxide slips and then glaze either with white or clear glazes. The slips I currently use include bronze (manganese oxide, cobalt and iron oxide), blue (cobalt with manganese oxide), green (copper carbonate and oxide), red (iron oxide). I am now wondering how to get turqoise, mustard/yellow and other colours. Are other colours possible with basic and inexpensive ingredients? Thanks Martin
×