  1. Sylvia Mondloch

    Oxyprobe Axner vs Bailey

    I've had an Axner Oxyprobe about 20 years. It's always seemed rather finicky and fragile. I've replaced the platinum wire (ouch) a couple times. I've been firing without now for awhile but miss having one. The catalog description of the probe on the ( more pricey)Bailey sounds more sturdy. Wondering if anyone has experience with both.
  2. Sylvia Mondloch

    Oxyprobe Axner vs Bailey

    Thanks for the reply. That controller and set-up looks more high-tech then I'm familiar with. Sounds like protecting it from soda is a definite to-do for me.
  3. Sylvia Mondloch

    Oxyprobe Axner vs Bailey

    I like the idea of pulling the tube back into the wall. Should work since the wood/soda happens just towards the end of the firing anyway.
  4. Sylvia Mondloch

    Oxyprobe Axner vs Bailey

    Thanks for the reply. I'm firing a propane MFT car kiln. I often add a couple wood sticks with soda on them towards the end of a firing for added variation. I'm guessing that is adding to the deterioration of the platinum wire. I guess I have to decide if I can justify the ongoing cost for the added control.
  5. It's that time of the year when we evaluate our business practices. We sell almost 100% of our work through our home studio gallery. Taking credit cards over an Ameribanc reader has been going smoothly, but with all the add-ons charges it ran about 4.6% last year which seems high to me. We bought the Amazon square but it seems flimsy for desktop use in our shop. I also like having an immediate receipt to give the customer. We use QuickBooks accounting software and have looked a little into switching to them and their desktop reader but they'd want us to update to QuickBooks on-line which scares me a bit. I'm curious what others use who sell from their home shop.
×