  1. Thank you I will try again
  2. I have tried vinegar too , By the way
  3. I have tried vinegar too , By the way
  4. I am following with interest, I have watched the Britt video and while it's clear for a glaze that deadpan , it's not clear for a glaze that just thickens...i added sodium silicate and it gets thicker. I am dumbfounded. I read somewhere then when it thickens so much you can add more water, but Britt says it's a no no. I have tried Epsom salts too and the glaze already has 3% bentonite ...and it thickens ...Help?
×