  1. Glaze Question On Purchased Item

    Thanks all so much. I even get to tell the artist experts in my family. LOL. Happy Thanksgiving to all for taking a few minutes out of your day. Frank
  2. Hi. I apologize for such a 'newbie' post but both my mother and sister, both artists, are unable to answer my question. I purchased a ceramic sushi set for my 10 year old daughter as a gift, ordered online from an auction site. The ceramic pieces arrived intact with an intact clear outer glaze. The inner color glaze appears to have small spider-like cracks thoughout the pattern and is present in all the pieces of the set. It looks as if the central color layer fractured like a windshield everything else didn't (everything is smooth on the outside). I am not sure if this is part of the design and expected glazing process or if this is defective. Thanks for your input. I am attaching a pic of one dish. F
×