  1. Bisque firing

    Thank you so much for that. I will try it tomorrow.
  2. Bisque firing

    Stoneware and earthenware can be fired together for the bisque firing i.e. at around 1,000 degrees centigrade. Thank you so much for that. I will try it tomorrow.
  3. Bisque firing

    I share a studio with some friends in London. We recently acquired a secondhand electric kiln. We have a backlog of lots of stoneware to fire and a few terracotta pieces. Can we put them both in the kiln for bisque firing? Sorry to be so ignorant but we are beginners.
×