    You might try slicing almost all the way through the pot when it is almost leather hard, let it dry further then slice all the way through. Make sure you low fire for a couple hours...OR.... put it in your oven and take it from 100F to 350F in 3 hours....Slow drying will help it to not crack further . Cathy