  1. I am new to ceramics and have started working with cone 10 crystal glazes. I am trying to get red under the crystal glaze. I have tried adding copper oxide to the glaze firing it than putting it through reduction at 1700 F for 15 to bring out the red. It has not worked, I sometimes get a little pink but mostly tan. Should I try a red slip and where can I get a formula for it?