  1. Hi there, we do a lot of Raku in Aus. Last week we had a mixture of results with copper lustre, the ones that worked well had lots of sawdust put on them in the reduction bins for about 20mins then hosed. The ones with only newspaper on them turned out turquoise instead of copper red. Hope this helps. Lyn
  2. Hi there I teach ceramics in Aus. What we use for waterproofing is a product called "Bondcrete" from any hardware shops. To stop dirt and for easy cleaning for outdoor ceramics use it one third Bondcrete to two thirds water. For pots without glaze for more waterproofing try half bondcrete and half water. It dries clear, the more bondcrete you use the more shiny it will look. Hope this helps. Cheers Aussie Lyn
×