  1. Correcting Porcelain Recipe

    Thanks,John I really don't know how to find all those products! I live in Brazil, and here the places where they sell those materials don't know much about its chemistry, and I'm a begginer also... So I'll try my best to find all these 'low iron ball clay"... I do have the Potash feldspar, which I've used... What means thixotropic? Thanks for answering! Pat
  2. Porcelain Recipe

    Sorry! 35 percent!
  3. Porcelain Recipe

    Hi! Thanks for the tip, but what should I remove? to increase more 20% of clay, to make a recipe in porcentage, I'll need to remove some part of some elements... Thanks for answering! Bye, Pat
  4. Porcelain Recipe

    Hi, I'm trying to produce my own porcelain. I began with the most simple recipe 15% Caolin 15% white clay 60% feldspat 10% flint It's to cone 6 1.230° Celsius It stays really white but not to plastic, not flexible, it cracks when I try to bend into a plaster mold, and if I add more water, it turns into mud. What can I do to correct and have a more plastic porcelain so I can have a very thin wall. Hope someone can help me. Thanks, Pat
  5. Correcting Porcelain Recipe

    Thanks! Hope finding it!
  6. Hi, I'm trying to produce my own porcelain. I began with the most simple recipe 15% Caolin 15% white clay 60% feldspat 10% flint It's to cone 6 1.230° Celsius It stays really white but not to plastic, not flexible, it cracks when I try to bend into a plaster mold, and if I add more water, it turns into mud. What can I do to correct and have a more plastic porcelain so I can have a very thin wall. Thanks, Pat
×

Important Information

By using this site, you agree to our Terms of Use.