  1. Green Ware Cracks

    Thank you - you have confirmed another potter's thoughts on this. And thank you for the suggestions for reference material.
  2. A thrown cylinder shaped piece developed a vertical crack at the rim AFTER it dried to the green ware stage. Another thrown small bowl developed a vertical crack at the rim in glaze firing both pieces are 1/8" thick or less at the rims I'm using Alberta plainsman M370 clay. Any ideas why?