  1. Avery?

    If a receipe calls for AVERY what else can be substituted? Thanks
  2. It will melt and carbonise. I recently made a tray and the feet fell off during the bisque. I waxed the side that sits on the table, glazed the round feet and glazed the bottom of the tray. When I fired the glaze, it held perfectly with no glue involved. I used the waxed side to know which side to put on the kiln shelf and sat the tray on top. Hope this helps.
  3. Homebuilt Gas Kiln - Need Advice

    I suggest you use an angled (45 degrees) brick at the opposite side of the gas burner to deflect the heat up.
×