  1. Hi, can anyone give me a good recipe for a completely clear glaze for stoneware high temperature (1200 °C). It's to use over other colors of glaze, engobes... to protected drawings but one that does not alter the colors to much. The gloss one we currently use at the artschool makes pink clay look grey! after firing at high temperature. I'm looking for a gloss and a matted version. Thanks!
  2. has not set their status

  3. Cracks In Greenware

    I have used clear white vinegar (not wine vinegar) on cracks and works a treat!
×