  1. Bonjour ! During the firing of a wood kiln what color the smoke from the chimney should be ? Someone told me that a black smoke is the sign of humid wood. Is it true ? Merci !
  2. Casting Slip

    Bonjour tout le monde How can I re-use dry scraps of casting slip? Merci
  3. Stilts On Stoneware

    I think my english is not very good...! My concern is not about the stilts but about the plate fired on them...
  4. Bonjour tout le monde ! One of my students wants me to fire his cone 5 plates on stilts. I told him that they will distord. Do you think that it is possible to fire stoneware on stilts. Or is it only for earthenware and bone china ?