  1. handle "issues"

    Thank you so much for answering my question! I think you are both right - the mug body is too dry for the handle attachment. I have been assuming that I can leave the mugs out longer here as there is so much more moisture in the air... but you know what they say about assuming. I will work on a new batch of mugs this week and let you know how it goes! Thanks again.... prpotter
  2. Hello everyone, I am having problems with my mug handles pulling away from the pot. I have recently moved from a very dry climate to a much more humid one, so am surprised at this happening. I usually pull my handles, let them set up and then score/slip on to the mug. It seems that no matter how slowly I dry them it still happens. I am using Plainsman clay, M340 and M370. Any ideas as to what I am doing wrong? Thanks in advance prpotter
×