  1. Leopard Spot Shino Glaze-need a recipe for

    It is not an effect that is accomplished by glaze formula alone. It is also highly dependent on the application and the firing steps. It's rather complex but gives lovely effects when done right. I doubt that it would be a suitable addition to a community studio setting. Far too many variables involved. When done incorrectly, the results can be quite ugly and whole loads of ware can be ruined.
×