View in one of the side stoke ports during the firing. Note the wood laying right on the pieces.


Sign in to follow this  
From the album:

Images For Misc. Posts

  • 33 images
  • 0 comments
  • 30 image comments

Photo Information for Fushigigama SidestokeportFlames Summer2017


Recommended Comments

Woodfiring is THE absolute MOST expensive way to fire in most situations. Labor! Wood prep. Extra steps in loading like wadding everything. Lots of cleanup of the kiln and furniture after a firing. Wear and tear on the kiln and posts and shelves. More than the average "unsuccessful" pieces. And then oh yeah.... stoking labor for hours. Were crazy.

Share this comment


Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.