This handbuilt bottle form shows the marks left by Josh Query's "manmade "seashells". The mix is 50% plaster, 50% whiting, and salt water to mix the stuff up with. Josh wanted shapes of marks that were more rectilinear than what naturally happens with scallop shells.

 

Was fired in the spring 2017 firing of New Hampshire Institute of Art's #Fushigigama. Was in the last rear stack of shelves.


Copyright

© 2017 - Josh Query -all rights reserved
Sign in to follow this  
From the album:

Images For Misc. Posts

  • 33 images
  • 0 comments
  • 30 image comments

Photo Information for Josh Query's Bottle Form with "Manmade Shell Marks"

Taken with Canon Canon PowerShot SX160 IS

  • 5.3 mm
  • 1/1000
  • f f/5.0
  • ISO 200
View all photo EXIF information

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.