Sunrise sunset night light, colored translucent porcelain.
Night light made with translucent porcelain I've been developing that fires almost to a glass. Fired items come out of the kiln with an appearance similar to fused glass, no glaze necessary. Because of slumping the clay works best with flat items or ones supported during firing.