Tomato mug 1
Made as a gift for a local café - Julienne Tomatoes
Standard 300 brown clay, Stone White glaze, waterfall brown lining
Tomato: Amaco velvet underglaze 2 coats radiant red and leaf green, waxed over for glaze dipping