"Harbinger of Hope Series", 2010, Cone 10, Stoneware, Gas/Reduction/Salt Fired, Tenmoku Glaze, Rutile Stain, Red Iron Oxide Stain, Dimensions (From Left) 21" x 5" X 21.5", 19" X 8" X 18", 13" X 5" X 12.5", 9.25" X 6" X 8.5".