glaze that settles rock-like quickly
September 29, 2023
glaze that settles rock-like quickly
HI all: I mixed a new glaze sample today. Have been looking for a good cone 5-6 white, and found this one on Glazy. Silica 31 Fer Frit 30 Custer feldspar 28 Whiting 14 EPK