I need help from you experienced heads. I usually use white stoneware and fire to cone 6 but have decided to try out some ideas using brown clay (Electric Brown from Laguna) - at the same temperature. I would like a clear glaze which results in a nice rich color from the underlying clay, but a friend was showing me a pot he had just finished yesterday using a different brown clay. Where the pot was not glazed (footring) the color was a lovely lively red/brown but where it had been covered wit
I need help from you experienced heads. I usually use white stoneware and fire to cone 6 but have decided to try out some ideas using brown clay (Electric Brown from Laguna) - at the same temperature. I would like a clear glaze which results in a nice rich color from the underlying clay, but a friend was showing me a pot he had just finished yesterday using a different brown clay. Where the pot was not glazed (footring) the color was a lovely lively red/brown but where it had been covered wit