Hi,
A while ago I was looking through the book "Glazes cone 6" by Michael Bailey, and I saw a picture of a beautiful rust red platter and it's glaze recipe. So naturally I had to mix that glaze.... which turned an ugly brown for me, naturally.
On the next page is a suggested test method of starting with the base and adding 1% increments of red iron ox starting with 0% and ending with 23%. I was determined to get this color and texture so I did all of that work.... All brown. I was disg