Wind n Wing Posted April 21, 2011 Report Share Posted April 21, 2011 I want to make a support similar to those used to fire beads. No problem making the stilts but am unsure of what wire to use for supporting the beads or other hanging objects. I make windchimes and want to edge glaze some of my leaves so something that wont sag is paramont. As mentioned in the topic title I fire to cone 6. Any suggestions would be appreciated. Thanks, RJ Link to comment Share on other sites More sharing options...
Guest HerbNorris Posted April 22, 2011 Report Share Posted April 22, 2011 Try these places : http://www.kanthal.com/products/materials-in-wire-and-strip-form/wire/resistance-heating-wire-and-resistance-wire/ http://www.nationalartcraft.com/subcategory.asp?gid=10&cid=172&scid=451 http://www.resistancewire.com/mainpage.php?page=home Link to comment Share on other sites More sharing options...
Wind n Wing Posted April 22, 2011 Author Report Share Posted April 22, 2011 Try these places : http://www.kanthal.c...esistance-wire/ http://www.nationala...id=172&scid=451 http://www.resistanc...e.php?page=home Thanks Herb. I probably should have used the term rods instead of wire. The nationala site looks promising. Will be making a call to them in the morning. RJ Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.