Thought I'd share a success story here with my Terra Sigillata recipe. Everything I've ever read says that you need sodium silicate or sodium carbonate but it seems that Tetrasodium EDTA - aka Jet-Dry works as well.

 

3 parts Clay

1 part water

2 teastpoons Jet-Dry

 

I used a small bottle to mix up a test batch as I wasnt sure that it would work at all. Previous attempts at using Calgon were unsuccessful as I read that the old recipe containing phosphates was changed.

 

image9.jpg?w=300&h=300

 

So, if you dont have sodium silicate or sodium phosphate handy you can give this a try and see if it works for you.

 

Full post here - https://dreamsofearth.wordpress.com/2015/05/24/terra-sigillata/

Share this post


Link to post
Share on other sites

Oops! I meant to say 1 parts clay 3 parts water. I filled the bottle 3/4 of the way with water and filled up the rest with clay and then left just enough room for 2 teaspoons'ish Jet-Dry.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.