I want to start using Pilcher's slip on my sculptural pieces. It is a cone 04-10 recipe. What's the best plan to begin converting this into a vitreous recipe at cone 5/6?

Here's the recipe:

Ball clay 25, EPK 25, Flint 25, Cornwall Stone 12.5, Neph Sy 12.5

Add: Zircopax 5, Frit 3124 5

 

Thank you!

Tina

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.