Looking for a recipe. the color is about the same as copper that has oxidized. The result is a variegated color that varies from a turquoise to almost black spots.

 

 

i use this cone 6 glaze all the time... tried and true

 

 

 

TurquoiseNeph SyStrontiumFlintBall ClayLithiumTotal Also add:Copper CarbBentoniteEpson SaltComments:Very bright. Very turquoise, Matt, breaks black. Moves a lot if applied too thick. Create rough antique look a like texture.