I always see lots of colorful crystallines on colorful bases.

Does anyone know if it is possible to develop white (or colored) crystallines on a trasparent base, so that where there are no crystallines it is possible to see the clay body ?

 

 

Yep, Just don't add colorants. Should work with just about any crystalline formula.