JohnP 3 Posted October 5, 2014 Report Share Posted October 5, 2014 I am firing some work that is glazed cone 6 on the inside with just colored slips and an oxide wash on the outside i need to fire to cone six and was hoping to put the decal on the colored slips during this firing if i do a thin glaze wash or 3124 wash could i put the decal on top so it has some flux to adhere it or could i put the decal on and thin wash over it. The image is not detailed but i dont want it to rub off or fire out. Thank you Jp Link to post Share on other sites