I made a honey dipper and a spoon, each for the first time, but I don't know how to glaze fire them.  I've seen pictures of stoneware spoons and ladles online, and the pictures don't show holes (from hanging on a jewelry rack, for instance), so how are they fired?  Is it simple and I'm just brain-tired?  I think I have "potter's block" anyway, if there is such a thing.  Haven't been able to work up much enthusiasm in almost a month.  Maybe knowing how to make some spoons would get me started again.

 

 

Share this post


Link to post
Share on other sites

Back when I made a ladel with every soup tureen I would wax a small spot on bottom (touch spot( on spoon end and one on handle end.

Then place that spot on a small piece of soft brick. after firing grind off any rough edges.These where cone 10 and about a foot long.

Mark

Share this post


Link to post
Share on other sites

I did the similar waxing as Mark but without the soft brick. The handle of the ladle s had a large loop at the end. it was pulled so the finger ridges provided stabiliity when I set it on the shelf on two waxed spots on the handles.no need to grind them afterward.

 

Marcia

Share this post


Link to post
Share on other sites

The thing with the soft brick is if the glaze sticks it breaks away easy and grinds up well. I usewd to make a lot of throwen ladels with pulled handles back in the day. The bigest issue I have with a cermic ladel or spoon is they are made to bust so so easy. I switched to very nice wooden ladels-now I do not make either form as they are slow sellers.

Mark

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.