Good morning friends:

Does anyone have experience with gluing pieces that have broken or fallen off during bisque firing? Here people sometimes use UHU glue to glue pieces on before dipping in glazes and then glaze firing.

 

I have done this successfuly with a tiny piece but does any body know if this works for sprigs or heavier pieces? I have a vase where i sculpted leaves and pears then I attached them. The pear fell off during bisque firing and i want to glaze. I actually already used E6000 on the piece but now I wonder if it will melt and fall before the glaze can secure it?

 

The piece is German stoneware and I want to use a cone 6 glaze.

Thank you

Rosemary

Link to post
Share on other sites

Hi Riorose,  **beware of weird edited notations that don't make sense!**<br>I have reattached pieces using a paperclay patch. I reattached a student's handle to a pitcher and after the last firing it was strong enough to use full of a liquid. The glue is not a good idea. You will need to re-bisque after patching with paperclay.<br><font color="#1C2837"><font face="arial, verdana, tahoma, sans-serif"><font size="2">repairing with paper clay:Try to make a a few tablespoons worth at a time. It molds so no need to make more until needed.Take some of your dried clay and pulverize it with a rolling pin or spoon. Try for a 1/4 cup.  In a container, soak toilet paper...maybe a couple of feet or a yard or so. Tear it up into small pieces and soak over night. Squeeze some of the water out of it. In a blender put the toilet paper mash, add some water so the toilet paper can be fluid, add a little vinegar (1/2-1 tsp or so) , some karo syrup (1/4-1/2 tsp or so) , a dash of sodium silicate (a drop or two) and then clay. Blend to a thick paste consistency. You want the clay to be the prime ingredient. The toilet paper can be 15-25% of the volume. By squeezing it, you can visualize this estimate.Before applying the paste, wet the bisque surface so it doesn't suck in the moisture from the paste too quickly.  You can even re-attach broken parts using this system. Re-bisque fire the repaired piece.</font></font></font><div><font class="Apple-style-span" color="#1C2837" face="arial, verdana, tahoma, sans-serif"><span class="Apple-style-span" style="font-size: small;">You can cut back on water and increase both the vinegar and karo syrup.</span></font></div><div><font class="Apple-style-span" color="#1C2837" face="arial, verdana, tahoma, sans-serif"><span class="Apple-style-span" style="font-size: small;"><br></span></font><font color="#1C2837"><font face="arial, verdana, tahoma, sans-serif"><font size="2">Marcia</font></font></font>

 

</div>

Link to post
Share on other sites

Re: Glue

If a small piece needs to be re-attached before a final glaze - there are a few variable that make or break it for me.

 

I sometimes glue the piece on and then glaze it well around the attached part. If the attached part is going to fall off based on gravity - then it may do so in the kiln. If it's something like a knob on top of a lid, then gravity will keep it there regardless of the glue.

If the attached piece is on the side hanging off - it never works, if it's sitting on something it works.

Best of luck.

 

Patricia Bridges

Bridges Pottery

www.bridgespottery.com

Link to post
Share on other sites

Re: Glue

If a small piece needs to be re-attached before a final glaze - there are a few variable that make or break it for me.

 

I sometimes glue the piece on and then glaze it well around the attached part. If the attached part is going to fall off based on gravity - then it may do so in the kiln. If it's something like a knob on top of a lid, then gravity will keep it there regardless of the glue.

If the attached piece is on the side hanging off - it never works, if it's sitting on something it works.

Best of luck.

 

Patricia Bridges

Bridges Pottery

www.bridgespottery.com

 

Link to post
Share on other sites

I tried the glue.....and learned the hard way that was not a good idea. So now I use paperclay to repair cracks and reattach handles, etc. I mix up about a quart of paperclay and keep it in an airtight container. I haven't had a problem with mold and have used from the same container for over a year. I put slip I have made using Magic Water in a blender, add shredded insulation purchased at a hardware store, and blend well. It's nice to have it already mixed when I need to make a repair.

Link to post
Share on other sites

I have used Amaco's Bisque Fix and can verify it works very well. I have even used it to repair green ware by mixing it with a small amount of slip for a color match with darker clays. It dries rock hard and fires well. Just follow the instructions, and do not sand or inhale.

 

Use this link to view: http://www.amaco.com/shop/product-322-amaco-bisque-fix.html

Link to post
Share on other sites
  • 8 months later...

Hi Riorose,  **beware of weird edited notations that don't make sense!**<br>I have reattached pieces using a paperclay patch. I reattached a student's handle to a pitcher and after the last firing it was strong enough to use full of a liquid. The glue is not a good idea. You will need to re-bisque after patching with paperclay.<br><font color="#1C2837"><font face="arial, verdana, tahoma, sans-serif"><font size="2">repairing with paper clay:Try to make a a few tablespoons worth at a time. It molds so no need to make more until needed.Take some of your dried clay and pulverize it with a rolling pin or spoon. Try for a 1/4 cup.  In a container, soak toilet paper...maybe a couple of feet or a yard or so. Tear it up into small pieces and soak over night. Squeeze some of the water out of it. In a blender put the toilet paper mash, add some water so the toilet paper can be fluid, add a little vinegar (1/2-1 tsp or so) , some karo syrup (1/4-1/2 tsp or so) , a dash of sodium silicate (a drop or two) and then clay. Blend to a thick paste consistency. You want the clay to be the prime ingredient. The toilet paper can be 15-25% of the volume. By squeezing it, you can visualize this estimate.Before applying the paste, wet the bisque surface so it doesn't suck in the moisture from the paste too quickly.  You can even re-attach broken parts using this system. Re-bisque fire the repaired piece.</font></font></font><div><font class="Apple-style-span" color="#1C2837" face="arial, verdana, tahoma, sans-serif"><span class="Apple-style-span" style="font-size: small;">You can cut back on water and increase both the vinegar and karo syrup.</span></font></div><div><font class="Apple-style-span" color="#1C2837" face="arial, verdana, tahoma, sans-serif"><span class="Apple-style-span" style="font-size: small;"><br></span></font><font color="#1C2837"><font face="arial, verdana, tahoma, sans-serif"><font size="2">Marcia</font></font></font>

 

</div>

 

BTW, I used your method of reattchment, re bisqued and then did the glaze fire. It held during the glaze fire although because of surface differences I needed to switch to an opaque glaze. It looks pretty good and I will use the method again if needed.

Link to post
Share on other sites
  • 2 months later...
  • 3 years later...

I tried the glue.....and learned the hard way that was not a good idea. So now I use paperclay to repair cracks and reattach handles, etc. I mix up about a quart of paperclay and keep it in an airtight container. I haven't had a problem with mold and have used from the same container for over a year. I put slip I have made using Magic Water in a blender, add shredded insulation purchased at a hardware store, and blend well. It's nice to have it already mixed when I need to make a repair.

When you say it's not a good idea, what happened when you used glue? Was it just that the piece was discoloured and didn't turn out very well or did it shatter in the kiln? The ears broke off a bunny I made, I have already glued them back on with uhu and was not going to glaze but if possible I would like to glaze. I use a communal kiln so I will not glaze the bunny if there is a chance that it will shatter and break other people's work, however, if it just that the finish isn't perfect, I don't mind. If you could let me know what happened for you that would be really helpful. Thanks!

Link to post
Share on other sites
  • 3 years later...
46 minutes ago, guycruls said:

I have the same issue, with a key difference: I am not planning on firing my biscuit again.

So I am looking for a glue, a strong glue, one that is appropriate for the material.

Many thanks

ya know I read this post and I am surprised any glue would withstand 2000 degrees. I obviously could be wrong but  I bet it didn't and the break was just sealed by glaze. If that's the case then all it did was hold it in place and its a weak flaw in pot. I would go with  paper clay or AMACO product if I were you.

Edited by Stephen
Link to post
Share on other sites

If you're dead set on not re-bisquing, you can still use the paper clay patch but you'll have to treat the piece as a once fire and go very slowly up to temp in the kiln. I'd suggest spraying your glaze on as well, as water from the glaze will re-wet the paper clay patch, and it could fall off. 

Link to post
Share on other sites
  • 1 month later...
  • 1 year later...

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.