Hi, I would like to try to "smoke" a piece.

So I think (maybe it's wrong :rolleyes: ) there's 2 way:

  1. I bisque fire, then I smoke fire, then I glaze with transparent glaze to keep the smoke effect
  2. I bisque fier, i fire earthware or stoneware, then I smoke fire

Friendly advice are welcome :P

Share this post


Link to post
Share on other sites

I'm no expert, but I think you will want to bisque fire, then just smoke the piece.  If you fire it again, hot enough to glaze it on top of the smoke, it will probably burn off the carbon.  So it would look as if you had not smoked it.  Others will probably know better.

Share this post


Link to post
Share on other sites

If you look at the top of the page and hit the Ceramic Arts Daily link you will find a ton of information on this under "pit firing".

 

http://ceramicartsdaily.org/ceramic-arts-daily-site-search/?cx=001510309991982260494%3Afn9s4gctyhs&cof=FORID%3A9&ie=UTF-8&q=pit+firing&sa.x=0&sa.y=0

 

Many other techniques use smoke to enhance the pieces ...enjoy!

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.