Hi,

I have been advised that a bodystain is no different as a glazestain and a bodystain can be used as a glazestain and vice versa.

I have fired a batch of testtiles with a pink Al-Mn bodystain mixed with 3 tipes of baseglazes I usually use for stains, and the result has been disappointing, with almost no coloration, and not a good melt.

I have been trying to find out what went wrong, and found on digital fire a sentence that sais that bodystains normally do not melt appropriately when used as glazestains.

I have also found in Matthes that if you use a Al-Mn pink stain you have to use a High viscosity glaze with a lot of Al2O3 and little ZnO and or B2O3.

One of the glazes has ZnO so that is logical.

The other glazes have no ZnO and B2O3 of highest 0.33, lowest 0.20.

 

What do you think went wrong?

 

Is there anybody who has experience in using bodystains as glazestains?

 

gr.

Lies

post-63611-0-80347700-1401377762_thumb.jpg

post-63611-0-13694500-1401377789_thumb.jpg

post-63611-0-80347700-1401377762_thumb.jpg

post-63611-0-13694500-1401377789_thumb.jpg

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.