clay from the cellar Posted November 27, 2010 Report Share Posted November 27, 2010 Hello - I have been looking for a mid range olive green glossy glaze for a long time with no success. I decorate many of my pots with a woodland and wildflower theme and would like to add this color to my glaze inventory. Is there anyone that would share a recipe or trade? Thanks so much. Link to comment Share on other sites More sharing options...
lakesidepottery Posted December 29, 2010 Report Share Posted December 29, 2010 We use a great olive green glaze at our studio and you are wellcome to use the recipe listed on our cone 6 glaze recipes. See some picture below. More pottery tips from Lakeside Pottery Same glaze applied thicker: Lakeside Pottery, Ceramic School & Studio 543 Newfield Avenue Stamford, CT 06905 203-323-2222 www.lakesidepottery.com Link to comment Share on other sites More sharing options...