I'm making some small vessels from slip cast porcelain, and really loving the soft matte look they get after being fired to bisque (1000celsius). Unfortunately when I fire to 1200celsius to finish them they get a rough sandy feel to them (feels like nails on a chalkboard) and lose the subtlely of colors/shrink etc.

 

My main issue is the sandy surface and I'm wondering if there are any issues with selling little planters as bisque? Is this generally frowned upon? The bisque doesnt leak water as such but it kind of bleeds through a little in spots but i could make it thicker.

 

OR- would it be better using another sort of clay that doesnt warp/shrink/and doesnt have that same rough texture? If so can someone recommend any? Plain earthenware? I would ideally like to make foodsafe versions eventually too which requires glaze obviously.

 

Any help would be greatly appreciated,

 

Jack

Share this post


Link to post
Share on other sites

Don't know the answers but I do know that when I use bisqued pots for myself arounfd the garden after a time, a number of years mind you, the pots start to flake and disintegrate. Takes a long time but....

My bisque was to teh same cone as you.

my clay was terracotta.

Share this post


Link to post
Share on other sites

Why not try some white earthenware slip for casting. It will mature at cone 04 (about 1050 Celsius) and I believe maintain some of that satiny finish you like. Water will still evaporate through it, but the clay will be mature.

 

Your porcelain slip is not mature at the bisque temp and will be a little less sturdy.

 

You can't really get around shrinkage. Most clay shrinks 10 - 15% on maturation. That's a generality - whatever clay you use should have the mature shrink % listed.

 

Experiment, it's fun and what it's all about!

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.