I am looking for a good stable clear liner glaze that does not have a tendency to craze. I found this in a past post with a reply from John Britt but its for cone 6

 

Mastering Cone 6 Glazes

GLOSSY CLEAR LINER cone 6

20.00 G-200 Potash Feldspar

20.00 Ferro 3134

15.00 Wollastonite

20.00 EPK China Clay

6.00 Talc

19.00 Silica

 

Does anyone know its range. If I take it to cone 7 - 8 will it still be stable? I am really searching for a good stable non crazing clear liner type glaze for this temperature.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.