Hi there...

I'm pouring molds and using earthenware slip. can i reclaim the trimmings by letting them dry out adding water. then using it as clay for example press molding and applying to a thrown pot, with magic water. or could i just knock it back up into a pouring slip and add diffloculant  wrong spelling I know . hope you know what I'm talking about,cos I'm not sure if I do,I've also got a earthenware clay and the slip can I throw the dry trimming in together and make a clay, for press molding lol any help would be appreciated...

Share this post


Link to post
Share on other sites

Hi

 

Yes, you can reuse the trimmings as plastic clay for other projects and you can add up to 25% of it back into another slip batch as long as you have not scraped any plaster from your moulds into the trimmings as they will explode in the firing and pop out pieces from the clay surface.

 

 

 

Irene

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.