Anyone had experience throwing with paper clay? Perhaps someone could save me the trouble and mess of mixing up a batch to experiment with?

Also, am I correct that the shrinkage rate of the clay body would be unchanged by the addition of paper fibers/dust?

Share this post


Link to post
Share on other sites

I see paper clay as an option to avoid green strength issues under very specific circumstances. It tends to create issues with plasticity and movement that would likely be unfavorable for throwing. The shrinkage of the body would only be effected in cases of large amounts of fiber additions. The materials would act the same, but the aggregate would reduce the relative amount of clay shrinking.

 

What type of item are you making that you anticipate needing to throw paperclay?

Share this post


Link to post
Share on other sites

As I remember it is difficult to get home made paper clay to the proper consistency for throwing. You might be better off with a commercial one.

There are downsides to functional wares being made with paper clay. The burnt out fibers leave more holes for water to get in even after glazing. Concerns range from seepage to problems with 'dishwasher to microwave' type heating.

Share this post


Link to post
Share on other sites

If you are making some paper clay for throwing, work the body into a slip. Then add the pulp which should be beaten well and without lumps. I think it was TJR who used toilet paper pulp in his porcelain. I have linter sheets and also cellulose blow-in insulation. I think the shrinkage rate may be reduced somewhat, but what is your objective. Paperclay is a wonder for hand building.No so much advantage for throwing and may actually be a hindrance.It is recommended to fire paper clay a cone higher to mature the clay body.If you are using a specific cone and glazes, this could resent problems.

 

 

Marcia

Share this post


Link to post
Share on other sites

I have been doing some testing on paper clay. One thing I have noticed after mixing a fresh batch it works better for me the same day or the next day, after that it gets a bit wonky on the wheel, but is still good for hand building.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.