I have an old Gare kiln  about 3 cu/ft that I am planning on making a raku kiln out of.  Since I'm a little flush from good Christmas sales I want to buy a Ward burner.  Which of these burners do I want? 

 

"With 1-8 PSI, the MR750 Single System is rated at 54,365 to 153,768 BTU's,           The MR100 is rated at 68,347 to 193,303 BTU's.

 

Probably will run them on propane, have gas available but will wait to see how all goes learning to fire the kiln.  Have already bought a digital pyrometer. 

 

Thanks for the help.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.