Need Advice Quickly About Cold Weather/kiln Operation

Recommended Posts

The coldest weather I've seen with my kilns is around 25 degrees (F).  Kilns are enclosed carport with no wind blowing in .  In 25 degrees coldest room gets is about 40 degrees.  

 

Expecting a low of 11 degrees.  What temperature do I need to run kilns?  Seems like I read room temp needs to be 32 degrees (F).   What are the guidelines?

 

Kiln schedule is

 

Bisque kiln firing Monday morning - Outside Temp expected to be around 20 degrees

Glaze kiln firing Monday night - Outside Temp  15 degrees dropping to around 11degrees

Bisque kiln firing Tuesday night-  Outside Temp around 30 degees

Glaze kiln firing Wednesday morning Temperatures 35/47 .... back to normal

 

Should I just skip firing on those 2 days?

Share this post


Link to post
Share on other sites

Thanks Chilly.  It says "in cold weather raise the temperature of the kiln's switch box to at least 32 degrees (F) (0 degrees C) before operating with a space heater." (its 0 to 50 C like yours)

 

So as long as it's 32 degrees on controller temperature, you can fun kiln.   I suppose that once kiln starts, temperature will keep rising and ambient temperature in room has no effect?     Can't imagine these low temperatures wouldn't affect the kiln's firing  but  it seems it's only the temperature on the controller that matters?

Share this post


Link to post
Share on other sites

I ran mine when overnight low was predicted to be 3 deg C,  My kiln is in a greenhouse! The minimum inside temperature that night was 14 deg C and the max was about 20.  Windows were open for ventilation and power cable entry, so I guess the heat from the kiln will keep the controller warmer than otherwise.  Good luck.

Share this post


Link to post
Share on other sites

You need the controller temperature to be above freezing . . . so the electronics (thermocouples, relays, etc) work properly. Once kiln gets going, the controller box will stay warm. Your controller is a computer; it doesn't work well in extremes. So, it might be good to have a heater on at the controller level for a pre-firing warm up and then during the initial firing schedule. Similar to folks using a fan to keep the controller from overheating during summer and hot days.

Share this post


Link to post
Share on other sites

I was worried because it will be about 5 degrees here in north Georgia in the morning. My manual kiln (Kiln sitter) just turned off and is in cool down mode with all peeps in place. My basement my hit the 40's by morning. But this sounds mild compared to Colorado. My Skutt has 2 1/2 inch thick bricks. Will this temperature make things cool too fast?  Right now basement is about 60 f.

 

                                                                                                                    ja

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.