I have a question I hope those if you that use it can help answer. I have a sculpture that took me over a week to make and almost month to dry slowly. I was getting ready to paint on the underglaze decoration when I noticed a very fine hairline crack across the tip of one ear, all I can think is it got bumped at some point and I didn't notice it. I whipped up my first ever batch of Paperclay Slip, thank you everyone for posting your recipes! I used toilet paper, some of my dry clay body, a bit of water and some vinegar to make a thick slurry. I brushed this on the ear inside and out in several layers allowing it to dry in between. Now that it's dry can I clean it up and paint underglaze on it like I was planning to? Or should I gently clean and smooth the area bisque it THEN paint on the underglaze?

 

Thanks for your help!

 

Terry

Link to post
Share on other sites

Thank you everyone. I have brushed on several layers of the Paper clay slip drying between and have painted on the underglaze and it's drying. Since it was still damp when I loaded the kiln it's going to have to wait until the next kiln load to see if it survives the firing process.

 

Terry

Link to post
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.