I had a relay fail during a Cone 5 glaze firing. The temp reached 1800 degrees and fired 10 and a half hours. The glazes were under fired  and looked chalky but they do not come off. I have replaced the bad relay and my question is: do I re-glaze before re-firing, just re-fire, or do I just throw the stuff away? 

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.