You can spray a dipping, pouring or brushing glaze. If it is a commercial brushing glaze it probably has gums and flocculants added to it to make it thick. If this is the case then you can either water it down just enough so it sprays or you can use a deflocculant (sodium silicate or Darvan). Increasing the psi of the compressor also helps spray a thick glaze, I spray one of my glazes on when it is a yogurt consistency this way.

Share this post


Link to post
Share on other sites

I usually water down my glaze that I spray to a cream consistency and over compensate by spraying a few layers. Also make sure your glaze is mixed and screened really well so it does not clog up the spray gun.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.