Chris Campbell 1,226 Posted August 5, 2013 Report Share Posted August 5, 2013 One of the things I notice in a nearby art center, in my workshops and here on this forum is a definite desire to "Do it Right". Potters would love a clay that suits all needs, a glaze that fits this clay and techniques that work every time. ( Unfortunately that is a dream world ) The one thing no one wants to do is FAIL. Failure has become such a toxic notion that people want to avoid it at all costs. BUT ... I would bet that every experienced potter in the world has learned more from failure than they ever have from success. Open that kiln and see a load of ugly and after you pick yourself up, you can learn a lot about glazes. Get a drying rack full of s-cracks and you learn about throwing the bottom of a pot as well as the sides and top. Have a glaze run all over your shelf and you learn to put experiments on spill plates or bowls. Listen to a load ping all day and you learn about glaze fit. Fire the glaze recipe that looked so good elsewhere and find it looks nothing like that from your kiln and you learn about firing schedules. Might I propose the notion that failure is fine; it's a learning tool that is not to be avoided. Failure is a lifelong occupational hazard for any potter. If you are not failing, you are not trying anything new. I've been working in clay for a lot of years and as anyone who reads my blog can verify, I failed last week. I will likely fail at something this week and next week. Care to share a failure that resulted in a learning leap? Link to post Share on other sites
Benzine 1,173 Posted August 5, 2013 Report Share Posted August 5, 2013 My first classroom firing, once I started teaching, I had several pinch bowls, that exploded. From that, I learned to be patient with my drying and firing schedule. Link to post Share on other sites
Wyndham 98 Posted August 5, 2013 Report Share Posted August 5, 2013 Failure, let me see, ah putting the wrong cone in the kiln sitter, lesson learned "How to glaze high bisque pots, no fun but it works, sorta" Next, putting the wrong ingredient in a glaze recipe, lesson learned, "How to chip & Clean glaze from a shelf" Next failure,limiting myself to other peoples beliefs, lesson learned ":there is more myth than fact about how to make & glaze pottery, prove and verify everything to yourself, it's your life, health and well being" Failure is the best teacher, and success is hard work with no easy answers with plenty of failures along the way Now did I light that kiln or just turn on the gas, Wyndham. Link to post Share on other sites
OffCenter 87 Posted August 5, 2013 Report Share Posted August 5, 2013 Care to share a failure that resulted in a learning leap? Don't use an outhouse until you look under the seat. Jim Link to post Share on other sites
Diane Puckett 41 Posted August 5, 2013 Report Share Posted August 5, 2013 Not listen to that little voice that tells me not to do something. Sometimes it is common sense, sometimes intuition, but the little voice is always right. Every time I don't listen, another otherwise fine pot dies. Link to post Share on other sites
trina 21 Posted August 5, 2013 Report Share Posted August 5, 2013 Care to share a failure that resulted in a learning leap? Don't use an outhouse until you look under the seat. Jim Don't use an outhouse if you wear suspenders, and don't fry bacon with your shirt off. T Link to post Share on other sites
trina 21 Posted August 5, 2013 Report Share Posted August 5, 2013 Take notes so you can be sure the mistakes you make are always new ones. T Link to post Share on other sites
oldlady 2,808 Posted August 5, 2013 Report Share Posted August 5, 2013 don't try to explain color with words. it must be seen. Link to post Share on other sites
Marcia Selsor 1,905 Posted August 5, 2013 Report Share Posted August 5, 2013 My first solo kiln firing in college was all ash glazes ..on too thin. Ash glaze needs to be applied thicker. Learned that. Notes are great. I made a nice glaze with a mistake in my math but I had written it down. Good one there!There are 40 more years of those mistakes to help going forward. Thanks, Chris, for the reminder about how we learn much more from mistakes. Marcia Link to post Share on other sites
Claypple 30 Posted August 6, 2013 Report Share Posted August 6, 2013 I was just recently thinking how lucky I am WITH the mistakes! 1) Pulled the cylinder too fast once: got a beautiful curve! Looks great! 2) Another cylinder collapsed: I tucked it in and got a double bowl. Cannot repeat it again. 3) Pulled the corners of the slab too much. Wanted to smash it back to the ball, but wait ... doesn't it look like a color of the coat? (This is how the series of my "coat vases" started.) 4) Had some clay scraps, was about to toss it, but noticed it looked like a whale on the wave. Kept it. There is actually a test done by psychiatrists, called "Rorschach test". They show you inkblots that actually have no meaning and ask you what you see in them. They then analyze your interpretation. So what I see in crooked bowels or a bended plates of mine reminds me that test. The problem is, I am more successful when I make the mistakes! So, my question is: Do the professional artists still practice accidental art, or it is just a beginner's thing? Is your the most successful work was a result of your imagination (Jim, I mean WITHOUT taking hydrocodone/vicodin!) or it happened by accident? Link to post Share on other sites
Chris Campbell 1,226 Posted August 6, 2013 Author Report Share Posted August 6, 2013 I usually know where I am going with a design, but try to flow with the clay and follow happy accidents. Also called short attention span. Link to post Share on other sites
Benzine 1,173 Posted August 6, 2013 Report Share Posted August 6, 2013 Bob Ross said, "There are no mistakes, only happy accidents." Fun fact, Bob Ross was in the Air Force, and held positions, that required him to "Scream" at his subordinates. Imagine, if he would have kept the same persona for his TV show.....It could have involved him demanding that viewers do push ups, for messing up the placement of their "Happy(Disciplined) Little Tree". Link to post Share on other sites
Bob Coyle 116 Posted August 6, 2013 Report Share Posted August 6, 2013 Might I propose the notion that failure is fine; it's a learning tool that is not to be avoided. Failure is a lifelong occupational hazard for any potter. If you are not failing, you are not trying anything new. I've been working in clay for a lot of years and as anyone who reads my blog can verify, I failed last week. I will likely fail at something this week and next week. The trick is to progress enough so that the failures become much fewer than the successes. Of course if you are in the experiment mode then a few failures is generally always the prelude to any success. I worked as a cosmetic chemist and had to formulate a crystal clear, high sudsing glycerine soap. 85 formulations later I got an acceptable product. Link to post Share on other sites
Evelyne Schoenmann 264 Posted August 6, 2013 Report Share Posted August 6, 2013 Sometimes failures hurt because you have spent so much time to create an object and then..... Before firing, but in bisque state After cone6 firing The round upper part was apparently too heavy for the delicate foot >sigh< and part of the foot melted down, crushed by the heavy weight from above. Lesson learned! Evelyne Link to post Share on other sites
JLowes 29 Posted August 7, 2013 Report Share Posted August 7, 2013 Latest learning experiences, get to know your new kiln controller. I purchased a Skutt KM-1 stand alone kiln controller. The first three bisque firings had at least one pot explode. One was spectacular, as it took out four others in one way or another, and I could only find a few small parts of the offender that were still recognizable. I had candled them for 8 hours at 180 F, checked them visually at the end of the candle and still had a steam explosion. My walls/bottoms are generally thin and even enough to not have this problem, at least not when I was manually advancing the temperature, but apparently the engineers at Skutt chose a ramp speed that didn't work well with some of my pots. Apparently somewhere on a pot each time had some trapped water that took longer than 8 hours to get out. Now I am extra careful at floor/wall transitions, joins, etc. to be sure there are no areas where trapping could occur, and I leave the peeps out and crack the lid (was using Orton Vent running before.) The last bisque firing had no casualties. My fingers are still crossed however. The glaze firings have been less problematic, but trying to slow down near top temperature caused the kiln sitter to trip once so no nice crystallization from a slow cool. John Link to post Share on other sites
oldlady 2,808 Posted August 7, 2013 Report Share Posted August 7, 2013 have you asked skutt for their parameters? they would want to know about any problems. Link to post Share on other sites
Benzine 1,173 Posted August 7, 2013 Report Share Posted August 7, 2013 Latest learning experiences, get to know your new kiln controller. I purchased a Skutt KM-1 stand alone kiln controller. The first three bisque firings had at least one pot explode. One was spectacular, as it took out four others in one way or another, and I could only find a few small parts of the offender that were still recognizable. I had candled them for 8 hours at 180 F, checked them visually at the end of the candle and still had a steam explosion. My walls/bottoms are generally thin and even enough to not have this problem, at least not when I was manually advancing the temperature, but apparently the engineers at Skutt chose a ramp speed that didn't work well with some of my pots. Apparently somewhere on a pot each time had some trapped water that took longer than 8 hours to get out. Now I am extra careful at floor/wall transitions, joins, etc. to be sure there are no areas where trapping could occur, and I leave the peeps out and crack the lid (was using Orton Vent running before.) The last bisque firing had no casualties. My fingers are still crossed however. The glaze firings have been less problematic, but trying to slow down near top temperature caused the kiln sitter to trip once so no nice crystallization from a slow cool. John Eight hours at 180, and you still had explosions?! I generally go for four hours at 200 F, and seldomly have problems. Keep in mind, this is with student projects, which greatly vary, both in thickness, and the care, in which they were built. Link to post Share on other sites
Chris Campbell 1,226 Posted August 8, 2013 Author Report Share Posted August 8, 2013 "Might I propose the notion that failure is fine; it's a learning tool that is not to be avoided. Failure is a lifelong occupational hazard for any potter. If you are not failing, you are not trying anything new. I've been working in clay for a lot of years and as anyone who reads my blog can verify, I failed last week. I will likely fail at something this week and next week." Yes, I am totally on schedule! Link to post Share on other sites
Judd 0 Posted August 29, 2013 Report Share Posted August 29, 2013 My students and I filled our school kiln, and opened a world of mess. Horrible glazes. Horrible pinch pots. Horrible horrible horrible. But, that's what I told my students to expect. I explained that we might see great stuff, but we might see a mess, and that this was part of the learning experience. Every time we make art, we get better. So, we're pinching pots, throwing pots, and preparing glaze. Link to post Share on other sites
Bob Coyle 116 Posted August 29, 2013 Report Share Posted August 29, 2013 Why horrible glazes? You should at least have control over that, unless your are testing new formulations on the horrible pinch pots. Don't you do test tiles first? Link to post Share on other sites
Chris Campbell 1,226 Posted August 29, 2013 Author Report Share Posted August 29, 2013 Not to answer his question but I would imagine that many high school students would not be incredibly accurate about things like glaze thickness, or combinations etc. ... Yes, you can do test tiles ... most group studios i have been in have them looking fine ... but in order to get that result you have to repeat accurately. Link to post Share on other sites
Bob Coyle 116 Posted August 30, 2013 Report Share Posted August 30, 2013 Too true Chris... and not only high school students. Link to post Share on other sites
Kohaku 27 Posted September 7, 2013 Report Share Posted September 7, 2013 This is a 14 inch conga drum (greenware) that I kicked five feet across my studio while loading a bisque kiln. Kids- don't stash your greenware on the floor. Link to post Share on other sites
Evelyne Schoenmann 264 Posted September 8, 2013 Report Share Posted September 8, 2013 Awwwwww that hurts (the soul and the heart I mean, not the toe...). So sorry that happened to you, Kohaku. But: we live and learn. Evelyne Link to post Share on other sites
Pres 2,398 Posted September 9, 2013 Report Share Posted September 9, 2013 Ouch, big blow to your ego there, and a good lesson. I am feeling the failure thing a lot of late, as the change in clay bodies has had me stymied as to where to go next. I am taking a little time off to make some new glaze tests, and am redoing a series of pieces I had done in the darker clay in a tan clay until I get this under control. It has me wondering about bisque levels, glaze thicknesses and slip applications. These things I had taken for granted. So failure is frustrating, but it can be good especially when you make your way to the other side! Link to post Share on other sites
Recommended Posts
Archived
This topic is now archived and is closed to further replies.