I am quite new to glazing and am looking for tried and true recipes. I particularly want a good aubergine gloss glaze which fires at cone 6 oxidation. I am using stoneware clay. Any suggestions welcome!

 

 

Share this post


Link to post
Share on other sites

Hi VivK... The first thing to learn...there is NO such thing as a tried and true recipe.

 next thing to learn is to  google "aubergine gloss glaze"

 

From clayart site....

 

Eggplant Purple -- cone 6 oxidation

Kona F-4 feldspar 45.7
Flint 15.2
Talc 12.7
Gerstley Borate 12.9
Dolomite 9.0
EPK 4.5

add:
Bentonite 1.0
Cobalt Carb. 2.0
Manganese Carb. 5.0

You MUST Test it first... your results may and probably will vary. glaze components are different from place to place and even from year to year.

Share this post


Link to post
Share on other sites

The magnesium in the talc & dolomite pushes the cobalt over to the purple/lavender in the glaze along with the manganese.

The base glaze components always affect the way coloring oxide behave.

Wyndham

Share this post


Link to post
Share on other sites

thank you, i am running out of a dark purple i mixed from two glazes that were ugly alone but made a nice surface together.  a little pansy purple mason made it great.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.