I have been experimenting with making small tree branches from clay and paperclay. I use 1/8" to 1/4" branches from a contorta tree (also called "Old Man Walking Stick" because of its twisted, curled and multi-angled branch formation. I push wads of clay onto the limbs, covering them completely until the finished clay limb looks much like the original limb. Then I dry the clay limbs and fire them in an electric kiln. The branches burn out, leaving a narrow bore inside the ceramic branches. Unfortunately, while the branches look great, they're very fragile. I'm wondering if there isn't something that I can brush onto the ceramic branches after firing that will harden and make them less breakable. I remember reading about a product that was being used to hold concrete blocks together without mortar, simply by brushing it onto the surface of the blocks. Something like that is what I have in mind. Any suggestions???

Share this post


Link to post
Share on other sites

isculpt

clay breaks - keeps us in buseness.

I've repaired a lot of fragile hollow ware also had a friend do large hollow spears ( 6ft)....always problems, always going to break. If you are committed to clay vers metal try pouring a plastic resin inside. IT WILL NOT protect braches from breaking but easier to repair because you will have a inside surface to work against.

Share this post


Link to post
Share on other sites

isculpt

clay breaks - keeps us in buseness.

I've repaired a lot of fragile hollow ware also had a friend do large hollow spears ( 6ft)....always problems, always going to break. If you are committed to clay vers metal try pouring a plastic resin inside. IT WILL NOT protect braches from breaking but easier to repair because you will have a inside surface to work against.

 

 

That was my thought as well...rolleyes.gif

Share this post


Link to post
Share on other sites

isculpt

clay breaks - keeps us in buseness.

I've repaired a lot of fragile hollow ware also had a friend do large hollow spears ( 6ft)....always problems, always going to break. If you are committed to clay vers metal try pouring a plastic resin inside. IT WILL NOT protect braches from breaking but easier to repair because you will have a inside surface to work against.

 

 

That was my thought as well...rolleyes.gif

 

 

thanks for the suggestions...

Share this post


Link to post
Share on other sites

Cjris is right. Mkke some paper clay slip and dip your branches in that..building up layers of thickness. For a decent quantity you can get a bag of cellulose from the hardware store (blown -in insulation) and ad that to a clay body ...scraps soaked and blended into a slip consistency. Then ad the cellulose. Try for a mix of 15-25% cellulose to what you think your dry clay amount of the slip would be. Guesstimate volume.

Marcia

Share this post


Link to post
Share on other sites

The paper-clay is great for you when you are making the clay branches, but fired paper-clay is going to be the same strength or even less strong than regular clay. Since you are losing the branch surface when you cover it with clay or slip anyway, why not sculpt them out of paper-clay directly. You can start with a fuzzy yarn dipped in paper-clay slip which will be strong enough to hold the shape as you work on it. The fuzzy yarn strengthens the "branch" as you work on it and then burns out creating a matrix inside that retains strength. This is a trick I learned from a paper-clay workshop from Potters Council with Rosette Gault and Graham Hay. Or, better yet, why not incorporate those wonderful contorta branches into a mixed media piece with unfired paper-clay? See an example of one where I did just that in this community image which I just posted.

Share this post


Link to post
Share on other sites

Cjris is right. Mkke some paper clay slip and dip your branches in that..building up layers of thickness. For a decent quantity you can get a bag of cellulose from the hardware store (blown -in insulation) and ad that to a clay body ...scraps soaked and blended into a slip consistency. Then ad the cellulose. Try for a mix of 15-25% cellulose to what you think your dry clay amount of the slip would be. Guesstimate volume.

Marcia

 

 

Thanks for the suggestions. I am using paperclay, both purchased and homemade, but I haven't tried using it as a slip...

Share this post


Link to post
Share on other sites

The paper-clay is great for you when you are making the clay branches, but fired paper-clay is going to be the same strength or even less strong than regular clay. Since you are losing the branch surface when you cover it with clay or slip anyway, why not sculpt them out of paper-clay directly. You can start with a fuzzy yarn dipped in paper-clay slip which will be strong enough to hold the shape as you work on it. The fuzzy yarn strengthens the "branch" as you work on it and then burns out creating a matrix inside that retains strength. This is a trick I learned from a paper-clay workshop from Potters Council with Rosette Gault and Graham Hay. Or, better yet, why not incorporate those wonderful contorta branches into a mixed media piece with unfired paper-clay? See an example of one where I did just that in this community image which I just posted.

 

 

Thanks for all of your thoughts on the subject! I'm not sure I understand the difference between using a fuzzy yarn or the actual contorta branch in the finished piece, since they both leave a hollowed out interior. Thank you for sharing your mixed media piece. A sculptor friend calls me a "purist", but I want to create branches from clay rather than add real branches. I know the real ones are probably more durable, but I just like the idea of faux branches! The reason that I build around the contorta branch rather than sculpting the branches directly is that I like the four-directions twists and turns of the contorta, and I can't seem to get that exact look without a base to build on.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.