The term "food safe" has no reall "legal" definition. What most people mean is, "will this surface leach out anything harmful into food"?

 

 

While there are what might be called "home tests" ...such as using household vinegar and looking for surface or color changes, the only REAL way to know FOR SURE is having laboratory standard leach tests done. These tests are mildly destructive... if the surface is not stable. Meaning that it COULD potentially alter the piece a little.

 

Additionally, you need to know what you are testing FOR. The only lechates regulated in the USA (and the Statge of Calif.) are lead and cadmium compounds. Ther are others that COULD potentially be of concern.

 

Lab testing will cost you about $30-40 for tha basic test...and about an additional $10-30 per compound that you wish to have tested for. Plus the shipping of the piece back and forth.

 

When compared to drinking out of plastic bottles, microwaving in plastic containers , and using plastic food wraps..... usually pottery is of little concern. But few think of what the plastics are getting into foods.

 

best,

 

.............john

Share this post


Link to post
Share on other sites

The term "food safe" has no reall "legal" definition. What most people mean is, "will this surface leach out anything harmful into food"?

 

 

While there are what might be called "home tests" ...such as using household vinegar and looking for surface or color changes, the only REAL way to know FOR SURE is having laboratory standard leach tests done. These tests are mildly destructive... if the surface is not stable. Meaning that it COULD potentially alter the piece a little.

 

Additionally, you need to know what you are testing FOR. The only lechates regulated in the USA (and the Statge of Calif.) are lead and cadmium compounds. Ther are others that COULD potentially be of concern.

 

Lab testing will cost you about $30-40 for tha basic test...and about an additional $10-30 per compound that you wish to have tested for. Plus the shipping of the piece back and forth.

 

When compared to drinking out of plastic bottles, microwaving in plastic containers , and using plastic food wraps..... usually pottery is of little concern. But few think of what the plastics are getting into foods.

 

best,

 

.............john

 

 

Pretty much everything we humans do, is killing us slowly.

 

I guess the goal, is to not add to the list of things that is expediting the process.

Share this post


Link to post
Share on other sites

The term "food safe" has no reall "legal" definition. What most people mean is, "will this surface leach out anything harmful into food"?

 

 

While there are what might be called "home tests" ...such as using household vinegar and looking for surface or color changes, the only REAL way to know FOR SURE is having laboratory standard leach tests done. These tests are mildly destructive... if the surface is not stable. Meaning that it COULD potentially alter the piece a little.

 

Additionally, you need to know what you are testing FOR. The only lechates regulated in the USA (and the Statge of Calif.) are lead and cadmium compounds. Ther are others that COULD potentially be of concern.

 

Lab testing will cost you about $30-40 for tha basic test...and about an additional $10-30 per compound that you wish to have tested for. Plus the shipping of the piece back and forth.

 

When compared to drinking out of plastic bottles, microwaving in plastic containers , and using plastic food wraps..... usually pottery is of little concern. But few think of what the plastics are getting into foods.

 

best,

 

.............john

 

 

Well, in that case, if a glaze recipe dose not contain lead, cadmium, barium, manganese, or any other harmful material then is having leach testing for lead, cadmium, and the like pointless?

 

Darrel

Share this post


Link to post
Share on other sites
Guest JBaymore
Well, in that case, if a glaze recipe dose not contain lead, cadmium, barium, manganese, or any other harmful material then is having leach testing for lead, cadmium, and the like pointless?

 

Darrel,

 

Yes.

 

best,

 

.................john

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.