tman123 Posted Wednesday at 06:33 PM Report Share Posted Wednesday at 06:33 PM Hi, I have a cress E-18 kiln that is around 6 years old. It has probably been fired 30-40 times. There are some glaze drips on the bottom of the kiln and there is some cracking happening around the kiln floor. I want to get this kiln in better condition before I start using it again and I need advice on what to do. Should I fill in the cracks somehow? Should I get the glaze off the floor? Any help would be appreciated. Thank you. Quote Link to comment Share on other sites More sharing options...
Denice Posted yesterday at 12:17 AM Report Share Posted yesterday at 12:17 AM Paragon has a repair cement that you can use on the cracks. I am lazy so I use a simpler solution, I usually have a broken shelves laying around. I use to put it directly on the bottom, I have my kilns set up for the Skutt Enviorvent now and have that hole in the middle. I make sure it isn't covered, If the break is in the right place I can leave it on the bottom. If not I raise it with half inch stilts. I try to make it as sturdy and steady as I can, I am really building a new bottom. You can purchase a new bottom but that can get quite pricey. Vacuuming your elements and making sure there is no glaze on them is a good place to start. If you have a manual fire check your weight and clearance on your kiln setter. Denice Quote Link to comment Share on other sites More sharing options...
neilestrick Posted yesterday at 03:16 AM Report Share Posted yesterday at 03:16 AM I wouldn't mess with the floor. You'll never get it cemented back together in a way that will hold. Best thing to do is to put a piece of stiff sheet metal under it to support it so it doesn't fall apart on the stand. Pres 1 Quote Link to comment Share on other sites More sharing options...
Babs Posted yesterday at 06:44 AM Report Share Posted yesterday at 06:44 AM Yes, really vacuum for a six year old kiln it is pretty messy. I hope none of the stuff spitting or dropping onto the ledges housing the elements has had contact with the elements. After you vacuum well I'd turn on higb ,leave a little while, open it up to see if all the elements get red. Quote Link to comment Share on other sites More sharing options...
tman123 Posted 22 hours ago Author Report Share Posted 22 hours ago Thank you all. I got all the glaze I could off around the entire kiln and vacuumed it. I’m going to put a new thermocouple in as well. I appreciate all of your help. Hulk 1 Quote Link to comment Share on other sites More sharing options...