HenryBurlingame Posted September 18 Report Share Posted September 18 (edited) So this is my first time using an extruder. I finally bit the bullet and got a Scott creek 4” extruder mainly to make a lot of test tiles. However, I keep getting tearing along some of the edges of the forms (usually where there is a curve, see attached image). What is the best way to prevent this? Do I just need to use softer than normal clay? Thanks! Edited September 18 by HenryBurlingame Quote Link to comment Share on other sites More sharing options...
Min Posted September 18 Report Share Posted September 18 25 minutes ago, HenryBurlingame said: Do I just need to use softer than normal clay Yes. Piedmont Pottery, Rae Reich, HenryBurlingame and 2 others 5 Quote Link to comment Share on other sites More sharing options...